To read this content please select one of the options below:

Stress corrosion cracking of sensitized austenitic stainless steels in Kuwait petroleum refineries

A. Almubarak (Department of Chemical Engineering, College of Technological Studies, Shuwaik, Kuwait)
M. Belkharchouche (Department of Chemical Engineering, College of Technological Studies, Shuwaik, Kuwait)
A. Hussain (Department of Buildings and Energy, Kuwait Institute for Scientific Research, Safat, Kuwait)

Anti-Corrosion Methods and Materials

ISSN: 0003-5599

Article publication date: 23 March 2010

942

Abstract

Purpose

The purpose of this paper is to investigate stress corrosion cracking (SCC) for 304, 316, and 321 stainless steels in petroleum‐processing environments.

Design/methodology/approach

Sensitized austenitic stainless steels were subjected to a microstructure investigation and electrochemical test. Stressed sensitized 304, 316, and 321 stainless steels were selected and subjected to various environments that included polythionic acid, sour solution, and chloride solution that were prepared in the laboratory to simulate service environments in the petroleum refinery.

Findings

Microstructure investigation reveals more severe SCC in polythionic acid than in the sour and chloride solutions. Type 321 SS gives better resistance to SCC than do 304 and 316 SS in the three solutions. It is concluded that acidity of solutions has a relatively minor influence in promoting cracking. However, polythionic acid is found to be the primary causative agent.

Originality/value

The results demonstrated that SCC is more severe in polythionic acid than in chloride and sour solutions.

Keywords

Citation

Almubarak, A., Belkharchouche, M. and Hussain, A. (2010), "Stress corrosion cracking of sensitized austenitic stainless steels in Kuwait petroleum refineries", Anti-Corrosion Methods and Materials, Vol. 57 No. 2, pp. 58-64. https://doi.org/10.1108/00035591011028014

Publisher

:

Emerald Group Publishing Limited

Copyright © 2010, Emerald Group Publishing Limited

Related articles