Effects of trace elements Hf and Si on oxidation behavior of Co-Ni-Al-W-based superalloys at 900°C

Fanjie Zhou (Institute for Advanced Materials and Technology, University of Science and Technology Beijing, Beijing, China)
Chunmei Ma (Institute for Advanced Materials and Technology, University of Science and Technology Beijing, Beijing, China)
Yuheng Zhang (Institute for Advanced Materials and Technology, University of Science and Technology Beijing, Beijing, China)
Jialu Wang (Institute for Advanced Materials and Technology, University of Science and Technology Beijing, Beijing, China)
Huadong Fu (Institute for Advanced Materials and Technology, University of Science and Technology Beijing, Beijing, China)

Anti-Corrosion Methods and Materials

ISSN: 0003-5599

Article publication date: 19 July 2022

Issue publication date: 4 August 2022

125

Abstract

Purpose

This study aims to control the oxidation resistance of Co-based deformed superalloys by adding trace elements Hf and Si.

Design/methodology/approach

The effects and mechanism of trace elements Hf and Si on the oxidation behavior of Co-Ni-Al-W-based forged superalloys were investigated by cyclic oxidation at 900°C.

Findings

The results show that the addition of trace elements Hf and Si does not affect the type of surface oxides of Co-Ni-based superalloys, and the oxidation layers of the alloys are TiO2, spinel, Cr2O3, TaTiO4, Al2O3 and TiN from outside to inside. However, the addition of elements can affect the activity of Cr and Ti elements; decrease the formation of TiO2 and TaTiO4 layers, which are harmful to the oxidation performance; and then improve the oxidation resistance of the alloy.

Originality/value

The relevant research results can not only optimize the microalloying element content of Co-Ni-Al-W-based superalloys, but also provide a new perspective for the composition optimization design of superalloys.

Keywords

Acknowledgements

The authors would like to thank the financial support of National Major Science and Technology Projects of China (J2019-VI-0009–0123), Science Center for Gas Turbine Project (P2021-A-IV-001–002) and Key-area Research and Development Program of Guangdong Province (No. 2019B010943001).

Citation

Zhou, F., Ma, C., Zhang, Y., Wang, J. and Fu, H. (2022), "Effects of trace elements Hf and Si on oxidation behavior of Co-Ni-Al-W-based superalloys at 900°C", Anti-Corrosion Methods and Materials, Vol. 69 No. 5, pp. 532-539. https://doi.org/10.1108/ACMM-03-2022-2621

Publisher

:

Emerald Publishing Limited