Application of Lean approach for reducing weld defects in a valve component: a case study

Karthik Bharathi S. (Department of Production Engineering, National Institute of Technology Tiruchirappalli, Tiruchirappalli, India)
S. Vinodh (Department of Production Engineering, National Institute of Technology Tiruchirappalli, Tiruchirappalli, India)
Sriharsha Devarapu (Department of Production Engineering, National Institute of Technology Tiruchirappalli, Tiruchirappalli, India)
Goutham Siddhamshetty (Department of Production Engineering, National Institute of Technology Tiruchirappalli, Tiruchirappalli, India)

International Journal of Lean Six Sigma

ISSN: 2040-4166

Article publication date: 5 June 2017

1952

Abstract

Purpose

The purpose of the study reported in the paper is to apply a structured problem-solving approach based on the Lean approach to analyse weld defects and derive appropriate solutions.

Design/methodology/approach

Manufacturing organisations involved in welding fabrication are expected to reduce weld defects to attain competitive advantage. Weld defects need to be systematically analysed for valve performance enhancement. In this research study, Lean approach is used to reduce variations and waste by annihilating the root causes for failures that occur during submerged arc welding (SAW) process.

Findings

The deployment of solutions facilitated weld defect reduction and substantial financial savings for the organisation.

Research limitations/implications

The framework has been test-implemented for analysing variations and wastes generated in the SAW process. In future, studies could be conducted for assessing different welding processes.

Practical implications

The proposed Lean framework has been successfully implemented in a large-scale manufacturing unit involved in fabrication work.

Originality/value

Lean framework has been test-implemented in a large-scale manufacturing organisation involved in weld fabrication work.

Keywords

Citation

S., K.B., Vinodh, S., Devarapu, S. and Siddhamshetty, G. (2017), "Application of Lean approach for reducing weld defects in a valve component: a case study", International Journal of Lean Six Sigma, Vol. 8 No. 2, pp. 181-209. https://doi.org/10.1108/IJLSS-01-2016-0001

Publisher

:

Emerald Publishing Limited

Copyright © 2017, Emerald Publishing Limited

Related articles